RFT
Probes
Probes
for inspection of pipe and tubing are typically of the bobbin
(ID) variety. These probes use either a single or dual excitation
coil to develop an electromagnetic field through the pipe
or tube. The excitation coils are driven by alternating current.
The sensing coil or coils are located a few tube diameters away
in the remote field zone. Probes can be used in differential or
absolute modes for detection of general discontinuities, pitting,
and variations from the I.D. in ferromagnetic tubing. To insure
maximum sensitivity, each probe is specifically designed for the
inside diameter, composition, and the wall thickness of a particular
tube.

|
|