Liquid Gases
|
Longitudinal Velocity
|
Density
g/cm3
|
Acoustic Impedance
g/cm2-sec
x105
|
|
cm/m sec
|
in/m sec
|
|
Liquid Argon (-186° C)
|
.0837
|
.033
|
1.404
|
1.175
|
|
Liquid Argon (-189° C)
|
.0863
|
.034
|
1.424
|
1.229
|
|
Freon MF 21.1
|
.0799
|
.0315
|
1.485
|
1.187
|
|
Freon TF 21.1
|
.0968
|
.0381
|
1.574
|
1.524
|
|
Liquid Helium (-269° C)
|
.0180
|
.0071
|
.125
|
.023
|
|
Liquid Helium (-271.5° C)
|
.0231
|
.0091
|
.146
|
.034
|
|
Liquid Hydrogen (-252.7° C)
|
.113
|
.0445
|
.355
|
.401
|
|
Liquid Nitrogen (-197° C)
|
.0869
|
.0342
|
.815
|
.708
|
|
Liquid Nitrogen (-203° C)
|
.0929
|
.0366
|
.848
|
.788
|
|
Liquid Oxygen (-183.6° C)
|
.0971
|
.0382
|
1.143
|
1.11
|
|
Liquid Oxygen (-210° C)
|
.113
|
.0445
|
1.272
|
1.437
|