Home - General Resources - Material Properties Tables - UT

-

Powered Metal and Materials

 

Longitudinal Velocity

Shear

Velocity

Surface

Velocity

Density

g/cm3

Acoustic Impedance g/cm2-sec

x105

cm/ms

in/ms

cm/ms

in/ms

cm/ms

in/ms

Rene (Cabot)

R-41 (53NI-19Cr-11Co-10Mo)

.604

.2378

.32

.126

.297

.117

6.25

49.8

R-77 (55NI-15Co-15Cr)

.62

.2441

.329

.1295

.305

.12

7.92

49.1

R-80 (6.5NI-9.9Co-14Cr)

.594

.2339

.323

.1272

N/A

N/A

N/A

N/A

R-95 (6lNf-8Co-14Cr)

.597

.235

N/A

N/A

N/A

N/A

8.19

48.9

-60 Mesh

.589

.2319

N/A

N/A

N/A

N/A

8.08

47.6

-As-HIP'd

.605

.2382

.302

.1189

N/A

N/A

N/A

N/A

-Cast & Wrought

.597

.235

.294

.1157

N/A

N/A

8.19

48.9

- HIP'D & Forged

.594

.2339

N/A

N/A

N/A

N/A

N/A

N/A

-150 Mesh

.603

.2374

.32

.126

.297

.117

8.30

50.0

-As HIP'd

.613

.2413

.32

.126

N/A

N/A

N/A

N/A

Wrought

.607

.239

.321

.1264

.298

.117

8.22

49.9

-