Home - General Resources - Material Properties Tables - UT

-

Wood

 

Longitudinal Velocity

cm/m s

in/m s

Ash (Along Fiber)

.467

0.1839

Birch (Along Fiber)

.334

0.1315

Cork

.0500

0.0197

Douglas Fir (Cross Grain)

.14

0.0551

Douglas Fir (With Grain)

.480

0.189

Elm (Wood)

.140

0.0551

Maple (Along Fiber)

.411

0.1618

Oak

.447

0.176

Pine (Along Fiber)

.332

0.1307

Poplar (Along Fiber)

.428

0.1685

Sycamore (Along Fiber)

.446