Home - General Resources - Standards
 

Partial List of ASTM Specifications

Please note that this list of ASTM specifications is provided for general reference only and may not be complete or current. Reference to the release date of the specification has been intentionally left off so that this list will not be used to check for the latest version of the document. Information provided by ASTM International should be consulted to ensure accuracy. ASTM web site can be found at www.astm.org

  • A577/A577M, Standard Specification for Ultrasonic Angle-Beam Examination of Steel Plates.
  • A578/A578M, Standard Specification for Straight-Beam Ultrasonic Examination of Plain and Clad Steel Plates for Special Applications.
  • A745/A745M, Standard Practice for Ultrasonic Examination of Austenitic Steel Forgings.
  • A898/A898M, Standard Specification for Straight Beam Ultrasonic Examination of Rolled Steel Structural Shapes.
  • A880, Standard Practice for Criteria for Use in Evaluation of Testing Laboratories and Organizations for Examination and Inspection of Steel, Stainless Steel, and Related Alloys.
  • B 244, Measurement of Thickness of Anodic Coatings on Aluminum and Other Nonconductive Coatings on Nonmagnetic Basis Metals with Eddy-Current Instruments.
  • B 499, Measurement of Coating Thickness by the Magnetic Method: Nonmagnetic Coatings on Magnetic Base Metals.
  • B 457, Standard Test Method for Measurement of Impedance of Anodic Coatings on Aluminum.
  • B 548, Standard Test Method for Ultrasonic Inspection of Aluminum-Alloy Plate for Pressure Vessels.
  • B 594, Standard Practice for Ultrasonic Inspection of Aluminum-Alloy Wrought Products for Aerospace Applications.
  • B 773, Standard Guide for Ultrasonic C-Scan Bond Evaluation of Brazed or Welded Electrical Contact Assemblies.
  • C 1175, Standard Guide to Test Methods and Standards for Nondestructive Testing of Advanced Ceramics.
  • C 1331, Standard Test Method for Measuring Ultrasonic Velocity in Advanced Ceramics with Broadband Pulse-Echo Cross-Correlation Method.
  • C 1332, Standard Test Method for Measurement of Ultrasonic Attenuation Coefficients of Advanced Ceramics by Pulse-Echo Contact Technique.
  • C 1383, Standard Test Method for Measuring the P-Wave Speed and the Thickness of Concrete Plates Using the Impact-Echo Method.
  • C 805, Standard Test Method for Rebound Number of Hardened Concrete.
  • C 597, Standard Test Method for Pulse Velocity Through Concrete.
  • D1186, Nondestructive Measurement of Dry Film Thickness of Nonmagnetic Coatings Applied to a Ferrous Base.
  • D1400, Nondestructive Measurement of Dry Film Thickness of Nonconductive Coatings Applied to a Nonferrous Metal Base.
  • D 4015, Standard Test Methods for Modulus and Damping of Soils by the Resonant-Column Method.
  • D 4602, Standard Guide for Nondestructive Testing of Pavements Using Cyclic-Loading Dynamic Deflection Equipment.
  • D 5339, Standard Practice for Quality Assurance Plan for Structural Steel Fabrication for Highway Structures.
  • D 5641, Standard Practice for Geomembrane Seam Evaluation by Vacuum Chamber.
  • D 5820, Standard Practice for Pressurized Air Channel Evaluation of Dual Seamed Geomembranes.
  • D 5858, Standard Guide for Calculating In Situ Equivalent Elastic Moduli of Pavement Materials Using Layered Elastic Theory.
  • D 6087, Standard Test Method for Evaluating Asphalt-Covered Concrete Bridge Decks Using Ground Penetrating Radar.
  • D 6365, Standard Practice for the Nondestructive Testing of Geomembrane Seams using the Spark Tests.
  • E 94, Standard Guide for Radiographic Examination.
  • E 114, Standard Practice for Ultrasonic Pulse-Echo Straight-Beam Examination by the Contact Method.
  • E 125, Standard Reference Photographs for Magnetic Particle Indications on Ferrous Castings.
  • E 127, Standard Practice for Fabricating and Checking Aluminum Alloy Ultrasonic Standard Reference Blocks.
  • E 142, Standard Method for Controlling Quality of Radiographic Testing.
  • E 155, Standard Reference Radiographs for Inspection of Aluminum and Magnesium Castings.
  • E 164, Standard Practice for Ultrasonic Contact Examination of Weldments.
  • E 165, Standard Test Method for Liquid Penetrant Examination.
  • E 186, Standard Reference Radiographs for Heavy-Walled (2 to 4 1/2-in. (51 to 114-mm)) Steel Castings.
  • E 192, Standard Reference Radiographs for Investment Steel Castings of Aerospace Applications.
  • E 213, Standard Practice for Ultrasonic Examination of Metal Pipe and Tubing.
  • E 214, Standard Practice for Immersed Ultrasonic Examination by the Reflection Method Using Pulsed Longitudinal Waves.
  • E 215, Standard Practice for Standardizing Equipment for Electromagnetic Examination of Seamless Aluminum-Alloy Tube.
  • E 242, Standard Reference Radiographs for Appearances of Radiographic Images as Certain Parameters Are Changed.
  • E 243, Standard Practice for Electromagnetic (Eddy-Current) Examination of Copper and Copper-Alloy Tubes.
  • E272, Standard Reference Radiographs for High-Strength Copper-Base and Nickel-Copper Alloy Castings.
  • E 273, Standard Practice for Ultrasonic Examination of the Weld Zone of Welded Pipe and Tubing.
  • E 280, Standard Reference Radiographs for Heavy-Walled (4 1/2 to 12-in. (114 to 305-mm)) Steel Castings.
  • E 309, Standard Practice for Eddy-Current Examination of Steel Tubular Products Using Magnetic Saturation.
  • E 310, Standard Reference Radiographs for Tin Bronze Castings.
  • E 317, Standard Practice for Evaluating Performance Characteristics of Ultrasonic Pulse- Echo Examination Instruments and Systems Without the Use of Electronic Measurement Instruments.
  • E 329, Standard Specification for Agencies Engaged in the Testing and/or Inspection of Materials Used in Construction.
  • E 376, Standard Practice for Measuring Coating Thickness by Magnetic-Field or Eddy-Current (Electromagnetic) Test Methods.
  • E 390, Standard Reference Radiographs for Steel Fusion Welds.
  • E 408, Standard Test Methods for Total Normal Emittance of Surfaces Using Inspection-Meter Techniques.
  • E 426, Standard Practice for Electromagnetic (Eddy-Current) Examination of Seamless and Welded Tubular Products, Austenitic Stainless Steel and Similar Alloys.
  • E 427, Standard Practice for Testing for Leaks Using the Halogen Leak Detector (Alkali-Ion Diode).
  • E 428, Standard Practice for Fabrication and Control of Steel Reference Blocks Used in Ultrasonic Examination.
  • E 431, Standard Guide to Interpretation of Radiographs of Semiconductors and Related Devices.
  • E 432, Standard Guide for Selection of a Leak Testing Method.
  • E 433, Standard Reference Photographs for Liquid Penetrant Inspection.
  • E 446, Standard Reference Radiographs for Steel Castings Up to 2 in. (51 mm) in Thickness.
  • E 479, Standard Guide for Preparation of a Leak Testing Specification.
  • E 493, Standard Test Methods for Leaks Using the Mass Spectrometer Leak Detector in the Inside-Out Testing Mode.
  • E 494, Standard Practice for Measuring Ultrasonic Velocity in Materials.
  • E 498, Standard Test Methods for Leaks Using the Mass Spectrometer Leak Detector or Residual Gas Analyzer in the Tracer Probe Mode.
  • E 499, Standard Test Methods for Leaks Using the Mass Spectrometer Leak Detector in the Detector Probe Mode.
  • E 505, Standard Reference Radiographs for Inspection of Aluminum and Magnesium Die Castings.
  • E 515, Standard Test Method for Leaks Using Bubble Emission Techniques.
  • E 543, Standard Practice for Agencies Performing Nondestructive Testing.
  • E 545, Standard Test Method for Determining Image Quality in Direct Thermal Neutron Radiographic Examination.
  • E 566, Standard Practice for Electromagnetic (Eddy-Current) Sorting of Ferrous Metals.
  • E 569, Standard Practice for Acoustic Emission Monitoring of Structures During Controlled Stimulation.
  • E 570, Standard Practice for Flux Leakage Examination of Ferromagnetic Steel Tubular Products.
  • E 571, Standard Practice for Electromagnetic (Eddy-Current) Examination of Nickel and Nickel Alloy Tubular Products.
  • E 587, Standard Practice for Ultrasonic Angle-Beam Examination by the Contact Method.
  • E 588, Standard Practice for Detection of Large Inclusions in Bearing Quality Steel by the Ultrasonic Method.
  • E 592, Standard Guide to Obtainable ASTM Equivalent Penetrameter Sensitivity for Radiography of Steel Plates 1/4 to 2 in. (6 to 51 mm) Thick with X-Rays and 1 to 6 in. (25 to 152 mm) Thick with Cobalt-60.
  • E 650, Standard Guide for Mounting Piezoelectric Acoustic Emission Sensors.
  • E 664, Standard Practice for the Measurement of the Apparent Attenuation of Longitudinal Ultrasonic Waves by Immersion Method.
  • E 689, Standard Reference Radiographs for Ductile Iron Castings.
  • E 690, Standard Practice for In Situ Electromagnetic (Eddy-Current) Examination of Nonmagnetic Heat Exchanger Tubes.
  • E 703, Standard Practice for Electromagnetic (Eddy-Current) Sorting of Nonferrous Metals.
  • E 709 Standard Guide for Magnetic Particle Examination.
  • E 746, Standard Test Method for Determining Relative Image Quality Response of Industrial Radiographic Film.
  • E 747, Standard Practice for Design, Manufacture, and Material Grouping Classification of Wire Image
    QualityIndicators (IQI) used for Radiology.
  • E 748, Standard Practices for Thermal Neutron Radiography of Materials.
  • E 749, Standard Practice for Acoustic Emission Monitoring During Continuous Welding.
  • E 750, Standard Practice for Characterizing Acoustic Emission Instrumentation.
  • E 751, Standard Practice for Acoustic Emission Monitoring During Resistance Spot-Welding.
  • E 797, Standard Practice for Measuring Thickness by Manual Ultrasonic Pulse-Echo Contact Method.
  • E 801, Standard Practice for Controlling Quality of Radiological Examination of Electronic Devices.
  • E 802, Standard Reference Radiographs for Gray Iron Castings Up to 4 1/2 in. (114 mm) in Thickness.
  • E 803, Standard Test Method for Determining the L/D Ratio of Neutron Radiography Beams.
  • E 908, Standard Practice for Calibrating Gaseous Reference Leaks.
  • E 976, Standard Guide for Determining the Reproducibility of Acoustic Emission Sensor Response.
  • E 977, Standard Practice for Thermoelectric Sorting of Electrically Conductive Materials.
  • E 998, Standard Test Method for Structural Performance of Glass in Windows, Curtain Walls, and Doors Under the Influence of Uniform Static Loads by Nondestructive Method.
  • E 999, Standard Guide for Controlling the Quality of Industrial Radiographic Film Processing.
  • E 1001, Standard Practice for Detection and Evaluation of Discontinuities by the Immersed Pulse-Echo Ultrasonic Method Using Longitudinal Waves.
  • E 1002, Standard Test Method for Leaks Using Ultrasonics.
  • E 1003, Standard Test Method for Hydrostatic Leak Testing.
  • E 1004, Standard Practice for Determining Electrical Conductivity Using the Electromagnetic (Eddy-Current) Method.
  • E 1025, Standard Practice for Design, Manufacture, and Material Grouping Classification of Hole-Type Image Quality Indicators (IQI) used for Radiology.
  • E 1030, Standard Test Method for Radiographic Examination of Metallic Castings.
  • E 1032, Standard Test Method for Radiographic Examination of Weldments.
  • E 1033, Standard Practice for Electromagnetic (Eddy-Current) Examination of Type F-Continuously Welded (CW) Ferromagnetic Pipe and Tubing Above the Curie Temperature.
  • E 1065, Standard Guide for Evaluating Characteristics of Ultrasonic Search Units.
  • E 1066, Standard Test Method for Ammonia Colorimetric Leak Testing.
  • E 1067, Standard Practice for Acoustic Emission Examination of Fiberglass Reinforced Plastic Resin (FRP) Tanks/Vessels.
  • E 1079, Standard Practice for Calibration of Transmission Densitometers.
  • E 1106, Standard Method for Primary Calibration of Acoustic Emission Sensors.
  • E 1114, Standard Test Method for Determining the Focal Size of Iridium-192 Industrial Radiographic Sources.
  • E 1118, Standard Practice for Acoustic Emission Examination of Reinforced Thermosetting Resin Pipe (RTRP).
  • E 1135, Standard Test Method for Comparing the Brightness of Fluorescent Penetrants.
  • E 1139, Standard Practice for Continuous Monitoring of Acoustic Emission from Metal Pressure Boundaries.
  • E 1158, Standard Guide for Material Selection and Fabrication of Reference Blocks for the Pulsed Longitudinal Wave Ultrasonic Examination of Metal and Metal Alloy Production Material.
  • E 1161, Standard Test Method for Radiologic Examination of Semiconductors and Electronic Components.
  • E 1165, Standard Test Method for Measurement of Focal Spots of Industrial X-Ray Tubes by Pinhole Imaging.
  • E 1208, Standard Test Method for Fluorescent Liquid Penetrant Examination Using the Lipophilic Post-Emulsification Process.
  • E 1209, Standard Test Method for Fluorescent Liquid Penetrant Examination Using the Water-Washable Process.
  • E 1210, Standard Test Method for Fluorescent Liquid Penetrant Examination Using the Hydrophilic Post-Emulsification Process.
  • E 1211, Standard Practice for Leak Detection and Location Using Surface-Mounted Acoustic Emission Sensors.
  • E 1212, Standard Practice for Quality Control Systems for Nondestructive Testing Agencies.
  • E 1213, Standard Test Method for Minimum Resolvable Temperature Difference for Thermal Imaging Systems.
  • E 1219, Standard Test Method for Fluorescent Liquid Penetrant Examination Using the Solvent-Removable Process.
  • E 1220, Standard Test Method for Visible Penetrant Examination Using the Solvent-Removable Process.
  • E 1254, Standard Guide for Storage of Radiographs and Unexposed Industrial Radiographic Films.
  • E 1255, Standard Practice for Radioscopy E1316, Standard Terminology for Nondestructive Examinations.
  • E 1311, Standard Test Method for Minimum Detectable Temperature Difference for Thermal Imaging Systems.
  • E 1312, Standard Practice for Electromagnetic (Eddy-Current) Examination of Ferromagnetic Cylindrical Bar Product Above the Curie Temperature.
  • E 1315, Standard Practice for Ultrasonic Examination of Steel with Convex Cylindrically Curved Entry Surfaces.
  • E 1316, Standard Terminology for Nondestructive Examinations.
  • E 1320, Standard Reference Radiographs for Titanium Castings.
  • E 1324, Standard Guide for Measuring Some Electronic Characteristics of Ultrasonic Examination Instruments.
  • E 1359, Standard Guide for Evaluating Capabilities of Nondestructive Testing Agencies.
  • E 1390, Standard Guide for Illuminators Used for Viewing Industrial Radiographs.
  • E 1411, Standard Practice for Qualification of Radioscopic Systems.
  • E 1416, Standard Test Method for Radioscopic Examination of Weldments.
  • E 1417, Standard Practice for Liquid Penetrant Examination.
  • E 1418, Standard Test Method for Visible Penetrant Examination Using the Water-Washable Process.
  • E 1419, Standard Test Method for Examination of Seamless, Gas- Filled, Pressure Vessels Using Acoustic Emission.
  • E 1441, Standard Guide for Computed Tomography (CT) Imaging.
  • E 1444, Standard Practice for Magnetic Particle Examination.
  • E 1452, Standard Practice for Preparation of Calibration Solutions for Spectrophotometric and for Spectroscopic Atomic Analysis.
  • E 1453, Standard Guide for Storage of Media That Contains Analog or Digital Radioscopic Data.
  • E 1454, Standard Guide for Data Fields for Computerized Transfer of Digital Ultrasonic Testing Data
  • E 1475, Standard Guide for Data Fields for Computerized Transfer of Digital Radiological Test Data.
  • E 1476, Standard Guide for Metals Identification, Grade Verification, and Sorting.
  • E 1495, Standard Guide for Acousto-Ultrasonic Assessment of Composites, Laminates, and Bonded Joints.
  • E 1496, Standard Test Method for Neutron Radiographic Dimensional Measurements.
  • E 1543, Standard Test Method for Noise Equivalent Temperature Difference of Thermal Imaging Systems.
  • E 1570, Standard Practice for Computed Tomographic (CT) Examination.
  • E 1571, Standard Practice for Electromagnetic Examination of Ferromagnetic Steel Wire Rope.
  • E 1603, Standard Test Methods for Leakage Measurement Using the Mass Spectrometer Leak Detector or Residual Gas Analyzer in the Hood Mode.
  • E 1606, Standard Practice for Electromagnetic (Eddy-Current) Examination of Copper Redraw Rod for Electrical Purposes.
  • E 1629, Standard Practice for Determining the Impedance of Absolute Eddy-Current Probes.
  • E 1647, Standard Practice for Determining Contrast Sensitivity in Radioscopy.
  • E 1648, Standard Reference Radiographs for Examination of Aluminum Fusion Welds.
  • E 1672, Standard Guide for Computed Tomography (CT) System Selection.
  • E 1695, Standard Test Method for Measurement of Computed Tomography (CT) System Performance.
  • E 1734, Standard Practice for Radioscopic Examination of Castings.
  • E 1735, Standard Test Method for Determining Relative Image Quality of Industrial Radiographic Film Exposed to X-Radiation from 4 to 25 MV.
  • E 1736, Standard Practice for Acousto-Ultrasonic Assessment of Filament-Wound Pressure Vessels.
  • E 1742, Standard Practice for Radiographic Examination.
  • E 1774, Standard Guide for Electromagnetic Acoustic Transducers (EMATs).
  • E 1781, Standard Practice for Secondary Calibration of Acoustic Emission Sensors.
  • E 1814, Standard Practice for Computed Tomographic (CT) Examination of Castings.
  • E 1815, Standard Test Method for Classification of Film Systems for Industrial Radiography.
  • E 1816, Standard Practice for Ultrasonic Examinations Using Electromagnetic Acoustic Transducer (EMAT) Techniques.
  • E 1817, Standard Practice for Controlling Quality of Radiological Examination by Using Representative Quality Indicators (RQIs)
  • E 1862-97(2002)e1 Standard Test Methods for Measuring and Compensating for Reflected Temperature Using Infrared Imaging Radiometers.
  • E 1888, Standard Test Method for Acoustic Emission testing of Pressurized Containers Made of Fiberglass Reinforced Plastic with Balsa Wood Cores.
  • E 1897, Standard Test Methods for Measuring and Compensating for Transmittance of an Attenuating Medium Using Infrared Imaging.
  • E 1901, Standard Guide for Detection and Evaluation of Discontinuities by Contact Pulse-Echo Straight-Beam Ultrasonic Methods.
  • E 1930, Standard Test Method for Examination of Liquid Filled Atmospheric and Low Pressure Metal Storage Tanks Using Acoustic Emission.
  • E 1931, Standard Guide for X-Ray Compton Scatter Tomography.
  • E 1932, Standard Guide for Acoustic Emission Examination of Small Parts.
  • E 1933, Standard Test Methods for Measuring and Compensating for Emissivity Using Infrared Imaging Radiometers.
  • E 1934, Standard Guide for Examining Electrical and Mechanical Equipment with Infrared Thermography.
  • E 1935, Standard Test Method for Calibrating and Meausring CT Density.
  • E 1936, Standard Reference Radiograph for Evaluating the Performance of Radiographic Digitization Systems.
  • E 1955, Standard Radiographic Examination for Soundness of Welds in Steel by Comparison to Graded ASTM E 390 Reference Radiographs.
  • E 1961, Standard Practice for Mechanized Ultrasonic Examination of Girth Welds Using Zonal Discrimination with Focused Search Units.
  • E1962, Standard Test Method for Ultrasonic Surface Examinations Using Electromagnetic Acoustic Transducer (EMAT) Techniques.
  • E 2001, Standard Guide for Resonant Ultrasound Spectroscopy for Defect Detection in Both Metallic and Non-Metallic Parts.
  • E 2002, Standard Practice for Determining Total Image Unsharpness in Radiology.
  • E 2003, Standard Practice for Fabrication of the Neutron Radiographic Beam Purity Indicators.
  • E 2023, Standard Practice for Fabrication of Neutron Radiographic Sensitivity Indicators.
  • E 2024, Standard Test Methods for Atmospheric Leaks Using a Thermal Conductivity Leak Detector.
  • E 2033, Standard Practice for Computed Radiology (Photostimulable Luminescence Method).
  • E 2075, Standard Practice for Verifying the Consistency of AE-Sensor Response Using an Acrylic Rod.
  • E 2076, Standard Test Method for Examination of Fiberglass Reinforced Plastic Fan Blades Using Acoustic Emission.
  • E 2096, Standard Practice for In Situ Examination of Ferromagnetic Heat-Exchanger Tubes Using Remote Field Testing.
  • E 2104, Standard Practice for Radiographic Examination of Advanced Aero and Turbine Materials and Components.
  • E 2191, Standard Test Method for Examination of Gas-Filled Filament-Wound Composite Pressure Vessels Using Acoustic Emission.
  • E 2192, Standard Guide for Planar Flaw Height Sizing by Ultrasonics.
  • E 2223, Standard Practice for Examination of Seamless, Gas-Filled, Steel Pressure Vessels Using Angle Beam Ultrasonic.
  • F 629, Standard Practice for Radiography of Cast Metallic Surgical Implants.
  • F 846, Standard Guide for Testing Performance of Amusement Rides and Devices.
  • F 914, Standard Test Method for Acoustic Emission for Insulated Aerial Personnel Devices.
  • F 1430, Standard Test Method for Acoustic Emission Testing of Insulated Aerial Personnel Devices with Supplemental Load Handling Attachments
  • F 1469, Standard Guide for Conducting a Repeatability and Reproducibility Study on Test Equipment for Nondestructive Testing.
  • F 1512, Standard Practice for Ultrasonic C-Scan Bond Evaluation of Sputtering Target-Backing Plate Assemblies.
  • F 1797, Standard Test Method for Acoustic Emission Testing of Insulated Digger Derricks.
  • G 62, Standard Test Methods for Holiday Detection in Pipeline Coatings.
  • G 158, Standard Guide for Three Methods of Assessing Buried Steel Tanks.

  • R0027- Standards Related to Nondestructive Testing Developed by ASTM Committees Other Than Committee E-7 (This is not an ASTM standard)